Welding Defects in Steel Structures: What Buyers Should Check

The common weld problems, why they happen, and which inspection records to ask your fabricator for.

Welding a built-up H beam for a steel structure building


Short answer: the weld defects that matter most in steel structures are porosity, slag inclusions, lack of fusion, undercut, overlap, cracks and undersized welds. Most are prevented by qualified procedures and welders, dry consumables, correct preheat, and inspection. As a buyer, you will rarely see these defects in photos; you control them by asking for the right documents and, on important projects, independent inspection.

Welding a built-up H beam for a steel structure building
Welding a built-up H beam for a steel structure building

This guide is for buyers of fabricated steel buildings and components. It does not replace a welding engineer's review on critical structures.

Common defects and causes

DefectWhat it isTypical causes
PorosityGas pockets in the weldDamp consumables, wind blowing away shielding gas, dirty plate
Slag inclusionSlag trapped between passesPoor cleaning between passes, wrong technique
Lack of fusion / penetrationWeld metal not fused with base metal or through the jointLow heat, wrong joint preparation, speed too high
UndercutGroove melted into the base metal at the weld toeCurrent too high, wrong angle
OverlapWeld metal rolls over the plate without fusingCurrent too low, slow travel
CracksHot or cold cracking in weld or heat-affected zoneMissing preheat on thick plate, hydrogen from damp rods, restraint
Undersized weldFillet leg smaller than designedNot checked against drawings

How good fabricators prevent them

  • Welding procedure qualification before production
  • Certified welders for each process and position
  • Consumables stored and dried as required
  • Preheat and interpass temperature control on thick plate
  • No outdoor welding in rain, snow or strong wind without protection
  • Automatic submerged-arc welding for long, critical seams on H beams
  • Inspection after welding: visual first, then ultrasonic (UT), magnetic particle (MT), penetrant (PT) or radiographic (RT) testing as specified

In China, welding of building steel follows GB 50661 (Code for welding of steel structures) and acceptance follows GB 50205 (Standard for acceptance of construction quality of steel structures). Your project may specify AWS D1.1 or EN ISO standards instead.

Gantry submerged arc welding machine for welded H beams
Gantry submerged arc welding machine for welded H beams

What to ask your fabricator for

  1. Welding procedure specifications for the main joints
  2. Welder qualification records
  3. Consumable certificates
  4. Visual inspection records and dimensional checks of weld size
  5. NDT reports (UT, MT, PT or RT) for the welds your engineer specifies
  6. Photos of typical welds before painting

Where to focus inspection

  • Full-penetration welds in column bases, knee joints and crane beams
  • Flange-to-web welds of built-up H beams
  • End plates of bolted connections
  • Any repaired weld

Third-party inspection

For export orders, many buyers hire an inspection company to witness tests and check welds before shipment. It is far cheaper than repairing welds on site abroad.

Our factory uses gantry submerged-arc and robotic welding for main members, and inspects welds by VT, MT, PT, UT and RT as specified. See our steel welding fabrication or ask for sample inspection records.

You cannot see most weld defects in a photo. Ask for welding procedures, welder qualifications and inspection reports instead.

Planning a steel building?

Send us the size, location and use of your building. Our engineers reply with a layout drawing and a priced material list you can compare line by line.

Request a free quote   WhatsApp +86 189 6830 7139